Plain Carbon Steel
0.18 - 0.23 C, 0.30 - 0.60 Mn, 0.040 P, 0.050 S
Annealed ( 1600 oF)
Tensile Strength (psi):
57250
Yield Strength (psi):
42750
Hardness (Bhn):
111
Hardened and Tempered (Tempering Range 1600 - 1600 oF)
Tensile Strength (psi):
64000 - 64000
Yield Strength (psi):
50250 - 50250
Hardness (Bhn):
131 - 131
0
0
The above values are taken from samples that were Normalized at 1600oF.
(Values of 0 are unknown or not applicable)
Date Entered: 4/22/01 Last Revised: 4/22/01