Alloy Steel
0.38 - 0.43 C, 0.75 - 1.00 Mn, 0.035 P (max), 0.040 S (max), 0.15 - 0.35 Si, 0.80 - 1.10 Cr, 0.15 - 0.25 Mo
Annealed ( 0 oF)
Tensile Strength (psi):
0
Yield Strength (psi):
0
Hardness (Bhn):
0
Hardened and Tempered (Tempering Range 0 - 0 oF)
Tensile Strength (psi):
110000 - 257000
Yield Strength (psi):
95000 - 238000
Hardness (Bhn):
230 - 510
0
0
Above values are based on Quenching and then Temering between 400 and 1200 deg F. The lower the tempering temperature, the greater the mechanical properties become.
(Values of 0 are unknown or not applicable)
Date Entered: 3/25/01 Last Revised: 3/25/01