Stainless Steel
23 - 26 Cr, 19 - 22 Ni, 0.25 C, 2.0 Mn, 1.5 - 3.0 Si, 0.045 P, 0.030 S
Annealed ( 0 oF)
Tensile Strength (psi):
10000
Yield Strength (psi):
50000
Hardness (Bhn):
170
Hardened and Tempered (Tempering Range 0 - 0 oF)
Tensile Strength (psi):
0 - 0
Yield Strength (psi):
0 - 0
Hardness (Bhn):
0 - 0
0
0
This material has a higher resistants to scale than AISI 310. Suited for severe cold heading or forming applications.
This is a Austenitic stainless steel.