Stainless Steel
23 - 28 Cr, 2.5 - 5 Ni, 0.8 C, 2.0 Mn, 0.75 Si, 0.040 P, 0.030 S, 1 - 2 Mo
Annealed ( 0 oF)
Tensile Strength (psi):
0
Yield Strength (psi):
0
Hardness (Bhn):
0
Hardened and Tempered (Tempering Range 0 - 0 oF)
Tensile Strength (psi):
0 - 0
Yield Strength (psi):
0 - 0
Hardness (Bhn):
0 - 0
0
0
Demonstrates simular corrosion resistance to AISI 316 type stainless steel but with better resistance to stress-corrosion cracking. This material is generally used for valve, pump and pipes.
General - This stainless is an Austenitic - Ferritic type.
Hardening - This material is capable of age hardening.
This is a Austenitic stainless steel.
(Values of 0 are unknown or not applicable)