Stainless Steel
17 - 20 Cr, 34 - 37 Ni, 0.08 C, 2.0 Mn, 0.75 - 1.50 Si, 0.040 P, 0.030 S
Annealed ( 0 oF)
Tensile Strength (psi):
0
Yield Strength (psi):
0
Hardness (Bhn):
0
Hardened and Tempered (Tempering Range 0 - 0 oF)
Tensile Strength (psi):
0 - 0
Yield Strength (psi):
0 - 0
Hardness (Bhn):
0 - 0
0
0
Due to it's good resistance to carburization, oxidation, and thermal shock, this material is commonly used for heat treating features.
This is a Austenitic stainless steel.
(Values of 0 are unknown or not applicable)
Date Entered: 4/13/01 Last Revised: 4/17/01