Stainless Steel
11.5 - 13.0 Cr, 0.15 C, 1.0 Mn, 0.5 Si, 0.040 P, 0.030 S, 0.60 Ni
Annealed ( 0 oF)
Tensile Strength (psi):
75000
Yield Strength (psi):
40000
Hardness (Bhn):
155
Hardened and Tempered (Tempering Range 400 - 1400 oF)
Tensile Strength (psi):
90000 - 195000
Yield Strength (psi):
60000 - 150000
Hardness (Bhn):
180 - 390
0
0
This grade of stainless is commonly used in steam turbines blades.
This is a Martensitic stainless steel.