Stainless Steel
12 - 14 Cr, 0.15 C, 1.25 Mn, 1.0 Si, 0.060 P, 0.15 S min, 0.060 Mo (optional)
Annealed ( 0 oF)
Tensile Strength (psi):
75000
Yield Strength (psi):
40000
Hardness (Bhn):
155
Hardened and Tempered (Tempering Range 400 - 14000 oF)
Tensile Strength (psi):
90000 - 195000
Yield Strength (psi):
60000 - 150000
Hardness (Bhn):
180 - 390
0
0
This is a free machining modification of type AISI 410 stainless. It is designed for heavier cuts.
This is a Martensitic stainless steel
(Values of 0 are unknown or not applicable)