Stainless Steel
16 - 18 Cr, 6 - 8 Ni, 0.15 C, 2.0 Mn, 0.75 Si, 0.045 P, 0.030 S
Annealed ( 2000 oF)
Tensile Strength (psi):
110000
Yield Strength (psi):
40000
Hardness (Bhn):
165
Hardened and Tempered (Tempering Range 0 - 0 oF)
Tensile Strength (psi):
125000 - 185000
Yield Strength (psi):
75000 - 140000
Hardness (Bhn):
265 - 400
0
0
Hight work-hardening rate. This material is used where high strength plus high ductility is required.
This stainless is an Austenitic Stainless.
Heat Treatment - This material is not hardened using heat treatment techniques. It is hardened by work hardening. This steel will work harden excessively.
This is a Austenitic stainless steel.