~Improvised Black Powder~WARNING! Certain text files and messages contained on this site deal with activities and devices which would be in violation of various Federal, State, and local laws if actually carried out or constructed. The webmasters of this site do not advocate the breaking of any law. Our text files and message bases are for informational/research purposes only. We recommend that you contact your local law enforcement officials before undertaking any project based upon any information obtained from this or any other web site. We do not guarantee that any of the information contained on this system is correct, workable, or factual. We are not responsible for, nor do we assume any liability for, damages resulting from the use of any information on this site.
Discuss Anarchy >>>
Black powder can be prepared in a simple, safe manner. It may be used as
blasting or gun powder.
Material Required
- Potassium Nitrate, granulated, 3 cups (3/4 liter)
- Wood charcoal, powdered, 2 cups
- Sulfur, powdered, 1/2 cup
- Alcohol, 5 pints (2-1/2 liters) (whiskey, rubbing alcohol, etc.)
- Water, 3 cups (3/4 liter)
- Heat source
- 2 buckets - each 2 gallon (7-1/2 litres) capacity, at least one of which is
heat resistant (metal, ceramic, etc.)
- Flat window screening, at least 1 foot (30 cm) square
- Large wooden stick
- Cloth, at leat 2 feet (60 cm) square
Procedure:
- Place alcohol in one of the buckets.
- Place potassium nitrate, charcoal, and sulfur in the heat resistant
bucket. Add 1 cup water and mix thoroughly with wooden stick until all
ingrediants are dissolved.
- Add remaining water (2 cups) to mixture. Place bucket on heat source and
stir until small bubbles begin to form.
CAUTION: DO NOT boil mixture. Be sure ALL mixture stays wet. If any is dry,
as on sides of pan, it may ignite!
- Remove bucket from heat and pour mixture into alcohol while stirring
vigorously.
- Let alcohol mixture stand about 5 minutes. Strain mixture through cloth to
obtain black powder. Discard liquid. Wrap cloth around black powder and
squeeze to remove all excess liquid.
- Place screening over dry bucket. Place workable amount of damp powder on
screen and granulate by rubbing solid through screen. NOTE: If granulated
particles appear to stick together and change shape, recombine entire batch
of powder and repeat steps 5 & 6.
- Spread granulated black powder on flat, dry surface so that layer about
1/2 inch (1-1/4 cm) is formed. Allow to dry. Use radiator, or direct
sunlight. This should be dried as soon as possible, preferably in an hour.
The longer the drying period, the less effective the black powder.
CAUTION: Remove from heat AS SOON AS granules are dry. Black powder isnow
ready to use.
Used in CBIV, '94
|
|